FWM™ 1537 alloy

FWM™ 1537 alloy is a low carbon wrought cobalt-chromium-molybdenum alloy that features high strength, ductility, wear resistance, corrosion resistance, and good biocompatibility.

 

Chemical composition

Composition

ASTM F1537
alloy 1
UNS R31537
%

Carbon 0.14 max
Chromium 26.0 - 30.0
Molybdenum 5.0 - 7.0
Nickel 1.0 max
Iron 0.75 max
Silicon 1.0 max
Manganese 1.0 max
Nitrogen 0.25 max
Cobalt Balance

 

Physical properties

  Metric English
Density 8.30 g/cm³ 0.300 lbs/in³
Modulus of Elasticity at 26 °C 241 Gpa 35 Mpsi
Thermal Conductivity at 21 °C 12.6 W/(m*°C) 87.4 BTU*in/(hr*ft²*°F)
Coefficient of Thermal Expansion

13.2 µm/(m*°C)

7.3 µin/(in*°F)

*Values calculated at 22 °C [72 °F]

 

Mechanical properties

Condition

Yield strength

Ultimate tensile strength Hardness
Rockwell C
Elongation
%

Annealed

552 MPa - 758 MPa
[80 ksi - 100 ksi]
1034 MPa - 1172 MPa
[150 ksi - 170 ksi]
30 - 35 > 25

Hard**

758 MPa - 896 MPa
[110 ksi - 130 ksi]
1172 MPa - 1344 MPa
[170 ksi - 195 ksi]
~ 40 > 30

*Values are typical and may not represent all diameters. Test methods will affect results.
**This material condition is similar to the ASTM condition "warm worked." The properties are similar, but the material is cold worked only. No thermal processing is used to achieve these properties.

 

FWM™ 1537 alloy

FWM™ 1537 alloy is a low carbon wrought cobalt-chromium-molybdenum alloy that features high strength, ductility, wear resistance, corrosion resistance, and good biocompatibility.

 

Chemical composition

Composition

ASTM F1537
alloy 1
UNS R31537
%

Carbon 0.14 max
Chromium 26.0 - 30.0
Molybdenum 5.0 - 7.0
Nickel 1.0 max
Iron 0.75 max
Silicon 1.0 max
Manganese 1.0 max
Nitrogen 0.25 max
Cobalt Balance

 

Physical properties

  Metric English
Density 8.30 g/cm³ 0.300 lbs/in³
Modulus of Elasticity at 26 °C 241 Gpa 35 Mpsi
Thermal Conductivity at 21 °C 12.6 W/(m*°C) 87.4 BTU*in/(hr*ft²*°F)
Coefficient of Thermal Expansion

13.2 µm/(m*°C)

7.3 µin/(in*°F)

*Values calculated at 22 °C [72 °F]

 

Mechanical properties

Condition

Yield strength

Ultimate tensile strength Hardness
Rockwell C
Elongation
%

Annealed

552 MPa - 758 MPa
[80 ksi - 100 ksi]
1034 MPa - 1172 MPa
[150 ksi - 170 ksi]
30 - 35 > 25

Hard**

758 MPa - 896 MPa
[110 ksi - 130 ksi]
1172 MPa - 1344 MPa
[170 ksi - 195 ksi]
~ 40 > 30

*Values are typical and may not represent all diameters. Test methods will affect results.
**This material condition is similar to the ASTM condition "warm worked." The properties are similar, but the material is cold worked only. No thermal processing is used to achieve these properties.